  1. IBetter Tank Scans of Bonded Sheets With B-Scan Section ViewsNov 2

Article I

Better Tank Scans of Bonded Sheets With B-Scan Section Views

By @weld-defect-insights

Better Tank Scans of Bonded Sheets With B-Scan Section Views When bonded sheets go through a test tank, each scan path must have a clear purpose. The team must know where sound should enter the metal or other test part. It also needs to know which flaws matter and which area must be covered. B-Scan Section Views is one piece of that plan. A good choice can help staff get a clear signal and trust the test. A weak choice can leave gaps that are hard to see on a bright